TY - THES A1 - Eckardt, Stefan T1 - Adaptive heterogeneous multiscale models for the nonlinear simulation of concrete N2 - The nonlinear behavior of concrete can be attributed to the propagation of microcracks within the heterogeneous internal material structure. In this thesis, a mesoscale model is developed which allows for the explicit simulation of these microcracks. Consequently, the actual physical phenomena causing the complex nonlinear macroscopic behavior of concrete can be represented using rather simple material formulations. On the mesoscale, the numerical model explicitly resolves the components of the internal material structure. For concrete, a three-phase model consisting of aggregates, mortar matrix and interfacial transition zone is proposed. Based on prescribed grading curves, an efficient algorithm for the generation of three-dimensional aggregate distributions using ellipsoids is presented. In the numerical model, tensile failure of the mortar matrix is described using a continuum damage approach. In order to reduce spurious mesh sensitivities, introduced by the softening behavior of the matrix material, nonlocal integral-type material formulations are applied. The propagation of cracks at the interface between aggregates and mortar matrix is represented in a discrete way using a cohesive crack approach. The iterative solution procedure is stabilized using a new path following constraint within the framework of load-displacement-constraint methods which allows for an efficient representation of snap-back phenomena. In several examples, the influence of the randomly generated heterogeneous material structure on the stochastic scatter of the results is analyzed. Furthermore, the ability of mesoscale models to represent size effects is investigated. Mesoscale simulations require the discretization of the internal material structure. Compared to simulations on the macroscale, the numerical effort and the memory demand increases dramatically. Due to the complexity of the numerical model, mesoscale simulations are, in general, limited to small specimens. In this thesis, an adaptive heterogeneous multiscale approach is presented which allows for the incorporation of mesoscale models within nonlinear simulations of concrete structures. In heterogeneous multiscale models, only critical regions, i.e. regions in which damage develops, are resolved on the mesoscale, whereas undamaged or sparsely damage regions are modeled on the macroscale. A crucial point in simulations with heterogeneous multiscale models is the coupling of sub-domains discretized on different length scales. The sub-domains differ not only in the size of the finite elements but also in the constitutive description. In this thesis, different methods for the coupling of non-matching discretizations - constraint equations, the mortar method and the arlequin method - are investigated and the application to heterogeneous multiscale models is presented. Another important point is the detection of critical regions. An adaptive solution procedure allowing the transfer of macroscale sub-domains to the mesoscale is proposed. In this context, several indicators which trigger the model adaptation are introduced. Finally, the application of the proposed adaptive heterogeneous multiscale approach in nonlinear simulations of concrete structures is presented. N2 - Das nichtlineare Materialverhalten von Beton ist durch die Entwicklung von Mikrorissen innerhalb der heterogenen Materialstruktur gekennzeichnet. In dieser Arbeit wird ein Mesoskalenmodell entwickelt, welches die einzelnen Bestandteile der Materialstruktur explizit auflöst und somit die Simulation dieser Mikrorisse erlaubt. Dadurch können die wirklichen physikalischen Vorgänge, welche das komplexe nichtlineare Verhalten von Beton verursachen, durch relativ einfache Materialformulierungen abgebildet werden. Für Beton wird auf der Mesoskala ein 3-Phasenmodell vorgeschlagen, bestehend aus groben Zuschlägen, Mörtelmatrix und Übergangszone zwischen Zuschlag und Matrix. In diesem Zusammenhang wird ein effizienter Algorithmus vorgestellt, welcher ausgehend von einer gegebenen Sieblinie dreidimensionale Kornstrukturen mittels Ellipsoiden simuliert. Im Mesoskalenmodell wird das Zugversagen der Mörtelmatrix durch einen Kontinuumsansatz beschrieben. Um Netzabhängigkeiten, welche durch das Entfestigungsverhalten des Materials hervorgerufen werden, zu reduzieren, kommen nichtlokale Materialformulierungen zum Einsatz. Risse innerhalb der Übergangszone zwischen Zuschlag und Matrix werden, basierend auf einem kohäsiven Modell, mittels eines diskreten Rissansatzes abgebildet. Die Verwendung einer neuen Nebenbedingung innerhalb der Last-Verschiebungs-Zwangsmethode führt zu einer Stabilisierung des iterativen Lösungverfahrens, so dass eine effiziente Simulation von Snap-back Phänomenen möglich wird. Anhand von Beispielen wird gezeigt, dass Mesoskalenmodelle die stochastische Streuung von Ergebnissen und Maßstabseffekte abbilden können. Da auf der Mesoskala die Diskretisierung der inneren Materialstruktur erforderlich ist, steigt im Vergleich zu Simulationen auf der Makroskala der numerische Aufwand erheblich. Aufgrund der Komplexität des numerischen Modells sind Mesoskalensimulationen in der Regel auf kleine Probekörper beschränkt. In dieser Arbeit wird ein adaptiver heterogener Mehrskalenansatz vorgestellt, welcher die Verwendung von Mesoskalenmodellen in nichtlinearen Simulationen von Betonstrukturen erlaubt. In heterogenen Mehrskalenmodellen werden nur kritische Bereiche auf der Mesoskala aufgelöst, während ungeschädigte Bereiche auf der Makroskala abgebildet werden. Ein wichtiger Aspekt in Simulationen mit heterogenen Mehrskalenmodellen ist die Kopplung der auf unterschiedlichen Längenskalen diskretisierten Teilgebiete. Diese unterscheiden sich nicht nur in der Größe der finiten Elemente sondern auch in der Beschreibung des Materials. Verschiedene Methoden zur Kopplung nicht übereinstimmender Vernetzungen - Kopplungsgleichungen, die Mortar-Methode und die Arlequin-Methode - werden untersucht und ihre Anwendung in heterogenen Mehrskalenmodellen wird gezeigt. Ein weiterer wichtiger Aspekt ist die Bestimmung kritischer Regionen. Eine adaptive Lösungsstrategie wird entwickelt, welche die Umwandlung von Makroskalengebieten auf die Mesoskala erlaubt. In diesem Zusammenhang werden Indikatoren vorgestellt, die eine Modellanpassung auslösen. Anhand nichtlinearer Simulationen von Betonstrukturen wird die Anwendung des vorgestellten adaptiven heterogenen Mehrskalenansatzes demonstriert. T2 - Adaptive heterogene Mehrskalenmodelle zur nichtlinearen Simulation von Beton T3 - ISM-Bericht // Institut für Strukturmechanik, Bauhaus-Universität Weimar - 2010,1 KW - Beton KW - Mehrskalenanalyse KW - Finite-Elemente-Methode KW - Nichtlineare Finite-Elemente-Methode KW - Schadensmechanik KW - Mehrskalenmodell KW - Adaptives Verfahren KW - concrete KW - multiscale method KW - finite element method KW - continuum damage mechanics KW - adaptive simulation Y1 - 2009 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20100317-15023 ER - TY - THES A1 - Bode, Kay-André T1 - Aspekte der kohäsiven und adhäsiven Eigenschaften von PCC T1 - Aspects of cohesive and adhesive properties of PCC N2 - Die Abkürzung PCC bezieht sie sich hier auf Polymer modified Cement Concrete, also mit Kunststoffen modifizierte Mörtel und Betone. Hierfür hat sich diese Abkürzung auch international durchgesetzt. Sie bezeichnet Baustoffe, die neben dem mineralischen Bindemittel Zement auch Kunststoffe enthalten. Zement und Kunststoff erzielen im späteren Mörtel bzw. Beton eine gemeinschaftliche Bindemittelwirkung. Wiederholter Gegenstand von Schadensfällen ist das Versagen des Haftverbundes zu anderer Bausubstanz. Da PCC häufig als dünne Schutzschicht auf vorhandenen Beton aufgetragen werden, führt ein Versagen der Adhäsion früher oder später auch zu einem Versagen dieser Schutzfunktion. Umgekehrt kann ein Versagen des Schutzes infolge von Rissen im PCC auch im Nachhinein zum Ablösen der Beschichtung führen. Ursächlich für dieses kohäsive Versagen sind dabei i. d. R. die Auswahl falscher bzw. nicht aufeinander abgestimmter Baustoffsysteme oder schlicht Verarbeitungsfehler. Das Ziel dieser Arbeit war es zu untersuchen, welchen Einfluss die kohäsiven und adhäsiven Eigenschaften von PCC auf deren Dauerhaftigkeit, insbesondere bei der Anwendung als Beschichtungsmaterial, haben. Dazu wurden vier maßgebliche Schwerpunkte bearbeitet. Eine zentrale Rolle für die Dauerhaftigkeit eines Beschichtungsmaterials spielt dessen Längenänderungsverhalten. Der Betrag der positiven und negativen Längenänderungen ist bestimmend für die Spannungen, die im Beschichtungsmaterial entstehen können. Sind die auftretenden Spannungen höher als die Zugfestigkeit des PCC erfolgt der Spannungsabbau durch Risse. Es kommt also zum Kohäsionsversagen im Mörtel. Wird der PCC als Beschichtungsmaterial genutzt, werden die Spannungen im Idealfall über die Verbundebene zum Beschichtungsuntergrund übertragen. Übersteigen dabei diese Spannungen die maximal aufnehmbaren Verbundspannungen, kommt es zum Adhäsionsversagen zwischen Beschichtung und Untergrund. In Modellversuchen werden die Effekte des Längenänderungsverhaltens kunststoffmodifizierter Zementsteine auf den Haftverbund zu einer Gesteinskörnung untersucht. Dadurch werden Rückschlüsse auf die Kohäsion innerhalb der PCC durch die Beschreibung des adhäsiven Verbundes zwischen Zementsteinmatrix und Gesteinskörnung gezogen. Neben der Längenänderung sind auch die Festigkeitseigenschaften der PCC bedeutsam für deren Dauerhaftigkeit. Es werden die Festigkeitseigenschaften kunststoffmodifizierter Mörtel und Betone nicht nur von der mechanischen Seite betrachtet. Der Focus liegt vielmehr auf der Beschreibung der durch die Kunststoffe beeinflussten kohäsiven Eigenschaften bei mechanischer Belastung. Es wird das Verhalten der polymeren Matrix nach einer Kurzzeitbelastung untersucht. Damit werden die Vorgänge, die letztlich zu einer Beeinflussung der Festigkeitseigenschaften führen, dargestellt. In diesem Zusammenhang wird auch der Einfluss der Temperatur auf die Festigkeit der PCC betrachtet. Die Untersuchung des Frost-Taumittel-Widerstandes mittels CDF- bzw. CIF-Verfahrens ist eine gute Möglichkeit, neben der Beurteilung der Dauerhaftigkeit auch Rückschlüsse auf die kohäsiven als auch, im mikroskopischen Maßstab betrachtet, die adhäsiven Eigenschaften der PCC zu ziehen. Damit ist gemeint, dass die Kohäsion von PCC durch deren adhäsive Eigenschaften zwischen kunststoffmodifizierter Zementsteinmatrix und Gesteinskörnern maßgeblich bestimmt wird. Einerseits kann bei starkem Abfall des relativen dynamischen E-Moduls von einer geringeren Kohäsion des PCC ausgegangen werden. Dies würde dann bei einem Mörtel eher zu Rissen führen, über die wiederum betonaggressive Medien eindringen können. Im Gegensatz dazu deutet ein konstant bleibender relativer dynamischer E-Modul auf eine hohe Kohäsion und damit, bei Anwendung des PCC als Beschichtungsmaterial, auf ein höheres adhäsives Versagensrisiko der Beschichtung hin. Andererseits stellt eine höhere Abwitterung, also sozusagen das schichtenweise kohäsive Versagen, eine Gefahr bei dünnen Beschichtungen dar. Dies könnte noch durch die Anwendung anderer Taumittel (z. B. organischer) verstärkt werden. Unter diesen Gesichtspunkten wurden Untersuchungen auf der Basis des CDF-Testes sowie zur Lösungsaufnahmefähigkeit der PCC durchgeführt. Der adhäsive Verbund von PCC zu Beton ist von vielen Faktoren abhängig. Bisher kaum betrachtet wurde die Art des Aufbringens oder der Einfluss der Probengeometrie bei Laborversuchen. Diese sowie der Einfluss einer Salzbelastung des Untergrundes bzw. der Beschichtung wurden untersucht. Ein Teil der durchgeführten Untersuchungen wurde im Rahmen des Teilprojektes B3 „Dauerhaftigkeit polymermodifizierter Mörtel und Betone“ des von der DFG geförderten Sonderforschungsbereiches 524 „Werkstoffe und Konstruktionen für die Revitalisierung von Bau-werken“ realisiert. N2 - Polymers were often combined with cementious mixtures to optimise different properties, e. g. the workability, the durability, the mechanical properties or the adhesion to other materials. Often it is unknown how the polymers affect in the PCC-matrix. Especially the reaktions under different stresses and strains are nondistinctive. Main points of the work are the shrinkage of PCC, the influence on the cohesion and adhesion inside of the material and the adhesion to other materials. This points were investigated under other views like durability properties (CDF-test) and mechanical load. The matrix of some polymer modified cement mortars (PCC) will be shown on a couple of SEM-pictures. Afterwards some selective mechanical and durability tests of PCC were introduced. The main properties of the investigated PCC were represented in some diagrams and tables. The stressed matrix will be visualised on SEM-pictures. On these pictures it will be imaginable, how different polymers act in the PCC-matrix. Some parts of the investigations were generated on the subproject B3 "Durability of Polymer modified Cement Concrete (PCC)" on the Collaborated Research Center 524 "Materials and Structures in Revitalisation of Buildings". KW - Betonzusatz KW - Beton KW - Kunstharzmodifizierter Zementbeton KW - Kohäsion KW - Adhäsion KW - Schwinden KW - Elastizitätsmodul KW - Kunststoffmörtel KW - Mörtel KW - Haftverbund KW - CDF-Verfahren KW - Taumittel KW - Mikroskopie KW - Kunststofffilme KW - cohesion KW - adhesion KW - polymer cement concrete KW - shrinkage KW - freeze-thaw-resistance Y1 - 2009 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20090513-14696 ER - TY - THES A1 - Tartsch, Enrico T1 - Bewertung der Dauerstandfestigkeit von dampfgehärtetem Porenbeton auf der Grundlage von Kurzzeitversuchen T1 - Prediction of the Sustained Load Strength of Autoclaved Aerated Concrete on a Short-term Basis N2 - Im Rahmen der Arbeit wird das Tragverhalten von dampfgehärtetem Porenbeton unter einachsiger Druckbeanspruchung untersucht. Ziel ist es, einen Zusammenhang zwischen makroskopischen Spannungs-Dehnungs-Beziehungen, beanspruchungsbedingten Strukturänderungen und der Dauerstandfestigkeit herzustellen. Die Dauerstandfestigkeit stellt im Sinne der Arbeit eine elementare Gefügeschwelle dar, durch sie wird das stabile vom instabilen Tragverhalten abgegrenzt. Der Zusammenhang zwischen Strukturänderungen und Spannungs-Dehnungs-Verhalten wird anhand mechanischer Modelle analysiert. Diese Untersuchungen liefern die konzeptionelle Orientierung für die durchzuführenden Laborversuche. Die experimentelle Basis der Arbeit bilden Kurzzeit- und Langzeitversuche an Porenbetonzylindern unter einachsiger Druckbeanspruchung. Es werden Probekörper von drei Porenbetonwerken untersucht. Um den Einfluss der Lastgeschichte aufzuzeigen, wird die Versuchsdauer zwischen einer Sekunde und mehreren Wochen variiert. Die Versuche werden mit unterschiedlichen Lastregimen durchgeführt: sowohl mit monoton gesteigerter Beanspruchung bis zum Versagen bzw. bis zum vorgesehenen Beanspruchungsniveau als auch mit niederzyklischer Beanspruchung. Die Messdaten werden unter Einbeziehung der dreidimensionalen Ansätze der Spannungs- und Deformationstheorie hinsichtlich des sphärischen und des deviatorischen Anteils des Spannungs- und Verformungszustandes ausgewertet. Diese auf die separate Betrachtung der Volumen- und Gestaltänderung gestützte Auswertung liefert zusätzliche Erkenntnisse hinsichtlich der Zuordnung von reversiblen und irreversiblen Verformungen zu den Teiltensoräquivalenten. Entsprechend den Versuchsergebnissen ändert sich die Kompressibilität des Porenbetons belastungsabhängig. Bereits kurzzeitige Überlastungen oberhalb der experimentell ermittelten Dauerstandgrenze sind von signifikanten Änderungen der Kompressionssteifigkeit begleitet. Das qualitative Tragverhalten des Porenbetons, das bei Beanspruchungen oberhalb der Dauerstandfestigkeit grundsätzliche Änderungen erfährt, lässt sich so bereits im Kurzzeitversuch abgrenzen. Zusätzliche Auswertungen für Normalbeton und selbstverdichtenden hochfesten Beton weisen auf analoges Verhalten hin. Auf der Basis der durchgeführten Untersuchungen werden Konzepte vorgestellt, mit denen die Dauerstandfestigkeit im Kurzzeitversuch, das heißt mit einer Versuchsdauer von wenigen Stunden, prognostiziert werden kann. Damit können Untersuchungen zur Dauerstandfestigkeit, die eine grundlegende Größe zur Beurteilung der Tragfähigkeit darstellt, routinemäßig durchgeführt werden. N2 - This thesis is concerned with the behaviour of autoclaved aerated concrete (AAC) when it is subjected to uniaxial compressive loads. The objective is to ascertain the relationship between textural changes, macroscopic stress-strain relations and the sustained load strength of the material itself. Throughout the thesis, the sustained load strength is considered as a basic threshold level, i.e. as the boundary between stable and unstable load-bearing behaviour. First, the effect of textural changes on the stress-strain behaviour was analysed on a theoretical basis with the aid of mechanical models. Based on the results, experimental tests were then planned. Short-term as well as long-term tests were carried out using cylindrical specimens made of AAC. Three different types of AAC were tested. Different load histories were used: monotonically increased loads and low-cycle loads with the load level increased step by step. Within the context of the test data analysis, three-dimensional textural responses are taken into account. Uniaxial loading is regarded as a special case of multi-axial loading. The decomposition of the stress tensor and strain tensor respectively opens up the opportunity to obtain more detailed information about elastic and inelastic material properties. It can be shown that compressibility of AAC undergoes load-dependent changes. Even short-term overloads lead to significant textural changes; these can be detected by analysing the bulk modulus. On this basis, it is possible to give clear statements about the sustained load strength of AAC. Additional tests carried out on normal-strength concrete and self-compacting concrete display similar behaviour. This study outlines a way of predicting sustained load strength on a short-term basis. As a result, it will be possible to carry out routine investigations into the sustained load strength in the future. T3 - Schriftenreihe des Instituts für Konstruktiven Ingenieurbau - 12 KW - Porenbeton KW - Beton KW - Tragverhalten KW - Dauerstandfestigkeit KW - Bruchverhalten KW - Experiment KW - Deformationsverhalten KW - zyklisch KW - Strukturänderung KW - elastische Eigenschaften KW - sphärisch KW - deviatorisch KW - Kompressibilität KW - textural changes KW - elastic properties KW - spherical KW - deviatoric KW - compressibility Y1 - 2008 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20080213-12926 ER - TY - THES A1 - Trümer, André T1 - Calcinierte Tone als Puzzolane der Zukunft - Von den Rohstoffen bis zur Wirkung im Beton N2 - Vor dem Hintergrund einer stetig wachsenden Nachfrage an Beton wie auch ambitionierter Reduktionsziele beim in der Zementproduktion anfallenden CO2 gelten calcinierte Tone als derzeit aussichtsreichste technische Neuerung im Bereich nachhaltiger Bindemittelkonzepte. Unter Ausnutzung ihrer Puzzolanität soll ein erheblicher Teil der Klinkerkomponente im Zement ersetzt werden, wobei der zu ihrer Aktivierung notwendige Energiebedarf vergleichsweise niedrig ist. Wesentliche Vorteile der Tone sind ihre weltweit nahezu unbegrenzte Verfügbarkeit sowie der äußerst geringe rohstoffbedingte CO2-Ausstoß während der Calcinierung. Schwierigkeiten auf dem Weg der Umsetzung bestehen allerdings in der Vielseitigkeit des Systems, welches durch eine hohe Varietät der Rohtone und des daraus folgenden thermischen Verhaltens gekennzeichnet ist. Entsprechend schwierig ist die Übertragbarkeit von Erfahrungen mit bereits etablierten calcinierten Tonen wie dem Metakaolin, der sich durch hohe Reinheit, einen aufwendigen Aufbereitungsprozess und eine entsprechend hohe Reaktivität auszeichnet. Ziel der Arbeit ist es daher, den bereits erlangten Kenntnisstand auf andere, wirtschaftlich relevante Tone zu erweitern und deren Eignung für die Anwendung im Beton herauszuarbeiten. In einem mehrstufigen Arbeitsprogramm wurde untersucht, inwieweit großtechnisch nutzbare Tone aktivierbar sind und welche Eigenschaften sich daraus für Zement und Beton ergeben. Die dabei festgestellte Reihenfolge Kaolinit > Montmorillonit > Illit beschreibt sowohl die Reaktivität der Brennprodukte als auch umgekehrt die Höhe der optimalen Calciniertemperatur. Auch wandelt sich der Charakter der entstandenen Metaphasen in dieser Abfolge von röntgenamorph und hochreaktiv zu glasig und reaktionsträge. Trotz dieser Einordnung konnte selbst mit dem Illit eine mit Steinkohlenflugasche vergleichbare Puzzolanität festgestellt werden. Dies bestätigte sich anschließend in Parameterversuchen, bei denen die Einflüsse von Rohstoffqualität, Calcinierung, Aufbereitung und Zement hinsichtlich der Reaktivitätsausbeute bewertet wurden. Die Bandbreite der erzielbaren Qualitäten ist dabei immens und gipfelt nicht zuletzt in stark unterschiedlichen Wirkungen auf die Festbetoneigenschaften. Hier machte sich vor allem die für Puzzolane typische Porenverfeinerung bemerkbar, sodass viele von Transportvorgängen abhängige Schadmechanismen unterdrückt wurden. Andere Schadex-positionen wie der Frostangriff ließen sich durch Zusatzmaßnahmen wie dem Eintrag von Luftporen beherrschen. Zu bemängeln sind vor allem die schlechte Verarbeitbarkeit kaolinitischer Metatone wie auch die für Puzzolane stark ausgeprägte Carbonatisierungsneigung. Wesentliches Ergebnis der Arbeit ist, dass auch Tone, die bisher als geringwertig bezüglich des Aktivierungspotentials galten, nutzbare puzzolanische Eigenschaften entwickeln können. So kann selbst ein stark verunreinigter Illit-Ton die Qualität von Flugasche erreichen. Mit stei-gendem Tonmineralgehalt sowie bei Präsens thermisch instabilerer Tonminerale wie Mont-morillonit und Kaolinit erweitert sich das Spektrum nutzbarer Puzzolanitäten bis hin zur hochreaktiven Metakaolin-Qualität. Damit lassen sich gute bis sehr gute Betoneigenschaften erzielen, sodass die Leistungsfähigkeit etablierter Kompositmaterialien erreicht wird. Somit sind die Voraussetzungen für eine umfangreiche Nutzung der erheblichen Tonmengen im Zement und Beton gegeben. Entsprechend können Tone einen effektiven Beitrag zu einer gesteigerten Nachhaltigkeit in der Baustoffproduktion weltweit leisten. KW - Beton KW - Ton Y1 - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20200214-40968 SN - 978-3-00-065011-6 ER - TY - THES A1 - Tatarin, René T1 - Charakterisieren struktureller Veränderungen in zementgebundenen Baustoffen durch akustische zerstörungsfreie Prüfverfahren N2 - Im Rahmen dieser Arbeit wird das Charakterisieren struktureller Veränderungen zementgebundener Baustoffe durch zwei auf dem Ultraschall-Transmissionsverfahren beruhenden Methoden der zerstörungsfreien Prüfung (ZfP) mit mechanischen Wellen vorgenommen. Zur kontinuierlichen Charakterisierung der Erstarrung und Erhärtung frischer zementgebundener Systeme wird ein auf Ultraschallsensoren für Longitudinal- und Scherwellen basierendes Messsystem in Kombination mit zugehörigen Verfahrensweisen zur Datenauswertung konzipiert, charakterisiert und angewandt. Gegenüber der bislang üblichen alleinigen Bewertung der Verfestigung anhand indirekter Ultraschallparameter wie Ausbreitungsgeschwindigkeit, Signalenergie oder Frequenzgehalt der Longitudinalwelle lässt sich damit eine direkte, sensible Erfassung der sich während der Strukturbildung entwickelnden dynamischen elastischen Eigenschaften auf der Basis primärer physikalischer Werkstoffparameter erreichen. Insbesondere Scherwellen und der dynamische Schubmodul sind geeignet, den graduellen Übergang zum Festkörper mit Überschreiten der Perkolationsschwelle sensibel und unabhängig vom Luftgehalt zu erfassen. Die zeitliche Entwicklung der dynamischen elastischen Eigenschaften, die Strukturbildungsraten sowie die daraus extrahierten diskreten Ergebnisparameter ermöglichen eine vergleichende quantitative Charakterisierung der Strukturbildung zementgebundener Baustoffe aus mechanischer Sicht. Dabei lassen sich typische, oft unvermeidbare Unterschiede in der Zusammensetzung der Versuchsmischungen berücksichtigen. Der Einsatz laserbasierter Methoden zur Anregung und Erfassung von mechanischen Wellen und deren Kombination zu Laser-Ultraschall zielt darauf ab, die mit der Anwendung des konventionellen Ultraschall-Transmissionsverfahrens verbundenen Nachteile zu eliminieren. Diese resultieren aus der Sensorgeometrie, der mechanischen Ankopplung und bei einer Vielzahl von Oberflächenpunkten aus einem hohen prüftechnischen Aufwand. Die laserbasierte, interferometrische Erfassung mechanischer Wellen ist gegenüber Ultraschallsensoren rauschbehaftet und vergleichsweise unsensibel. Als wesentliche Voraussetzung der scannenden Anwendung von Laser-Ultraschall auf zementgebundene Baustoffe erfolgen systematische experimentelle Untersuchungen zur laserinduzierten ablativen Anregung. Diese sollen zum Verständnis des Anregungsmechanismus unmittelbar auf den Oberflächen von zementgebundenen Baustoffen, Gesteinskörnungen und metallischen Werkstoffen beitragen, relevante Einflussfaktoren aus den charakteristischen Materialeigenschaften identifizieren, geeignete Prozessparameter gewinnen und die Verfahrensgrenzen aufzeigen. Unter Einsatz von Longitudinalwellen erfolgt die Anwendung von Laser-Ultraschall zur zeit- und ortsaufgelösten Charakterisierung der Strukturbildung und Homogenität frischer sowie erhärteter Proben zementgebundener Baustoffe. Während der Strukturbildung wird erstmals eine simultane berührungslose Erfassung von Longitudinal- und Scherwellen vorgenommen. Unter Anwendung von tomographischen Methoden (2D-Laufzeit¬tomo¬graphie) werden überlagerungsfreie Informationen zur räumlichen Verteilung struktureller Gefügeveränderungen anhand der longitudinalen Ausbreitungsgeschwindigkeit bzw. des relativen dynamischen Elastizitätsmoduls innerhalb von virtuellen Schnittebenen geschädigter Probekörper gewonnen. Als beton-schädigende Mechanismen werden exemplarisch der kombinierte Frost-Tausalz-Angriff sowie die Alkali-Kieselsäure-Reaktion (AKR) herangezogen. Die im Rahmen dieser Arbeit entwickelten Verfahren der zerstörungsfreien Prüfung bieten erweiterte Möglichkeiten zur Charakterisierung zementgebundener Baustoffe und deren strukturellen Veränderungen und lassen sich zielgerichtet in der Werkstoffentwicklung, bei der Qualitätssicherung sowie zur Analyse von Schadensprozessen und -ursachen einsetzen. N2 - In this research, structural changes of cement-based building materials are characterized using two ultrasonic transmission-based methods of non-destructive testing (NDT) with mechanical waves. For continuous characterization of setting and hardening of fresh cementitious materials a measurement system is designed, characterized and applied based on ultrasonic compressional and shear wave transducers in combination with associated data evaluation procedures. In contrast to common non-destructive testing of setting and hardening by means of solely indirect ultrasonic parameters such as pulse velocity, signal energy or frequency content of compressional waves, a direct sensitive recording of dynamic elastic properties can be achieved during the structure formation on the basis of primary physical material parameters. Especially, shear waves and the dynamic shear modulus are suitable to capture the gradual transition to a solid with exceeding percolation threshold in a sensitive manner and independent of air content. The development of dynamic elastic properties, the structure formation rates and the extracted discrete result parameters enable a comparative and quantitative analysis of the structural formation of fresh cementitious materials from a mechanical point of view. As an advantage, often unavoidable differences in the composition of test blends can be taken into account. The application of laser-based techniques for generation and detection of mechanical waves and their combination to laser-ultrasonics eliminates the disadvantages associated with the application of conventional ultrasonic through-transmission techniques. These result from sensor geometry, mechanical coupling and, in case of numerous surface points, due to a high inspection time and effort. Furthermore, the laser-based interferometric detection of mechanical waves is noisy and relatively insensitive compared to application of ultrasonic sensors. As an essential prerequisite, systematic experimental investigations of laser-induced ablative generation are carried out for the scanning application of laser-ultrasonics on cement-based building materials. These investigations contribute to the understanding of the excitation mechanism directly on the surfaces of concrete, natural aggregates and metallic targets and to the identification of relevant influencing factors from the characteristic material properties. By gathering optimized process parameters, the limitations of laser-ultrasonics to concrete are shown. Laser-ultrasonics is applied using compressional waves for time- and space-resolved characterization of the structure formation and homogeneity of fresh and hardened specimen of cement-based building materials. During the structure formation process, the simultaneous contactless acquisition of compressional and shear waves is carried out for the first time. With the implementation of tomographic methods (2D travel-time tomography) it is possible to obtain superposition-free information on the spatial distribution of microstructural changes by means of the longitudinal ultrasonic pulse velocity or the relative dynamic modulus of elasticity within virtual cross-sections of damaged specimens. The combined freeze-thaw de-icing salt attack as well as the alkali-silica reaction (ASR) are investigated as mechanisms of concrete damage. The methods of non-destructive testing developed within the scope of this study offer extended possibilities for the characterization of cement-based building materials and their structural changes and can be applied in a targeted manner in materials development, quality control and in analysis of damage processes and causes. KW - Beton KW - Hydratation KW - Ultraschall KW - Zerstörungsfreie Werkstoffprüfung KW - Lasertechnologie KW - Laser-Ultraschall KW - elastische Parameter KW - Tomographie KW - Strukturbildung KW - Dauerhaftigkeit Y1 - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20220215-45920 SN - 978-3-7369-7575-0 PB - Cuvillier Verlag CY - Göttingen ER - TY - THES A1 - Hanna, John T1 - Computational Fracture Modeling and Design of Encapsulation-Based Self-Healing Concrete Using XFEM and Cohesive Surface Technique N2 - Encapsulation-based self-healing concrete (SHC) is the most promising technique for providing a self-healing mechanism to concrete. This is due to its capacity to heal fractures effectively without human interventions, extending the operational life and lowering maintenance costs. The healing mechanism is created by embedding capsules containing the healing agent inside the concrete. The healing agent will be released once the capsules are fractured and the healing occurs in the vicinity of the damaged part. The healing efficiency of the SHC is still not clear and depends on several factors; in the case of microcapsules SHC the fracture of microcapsules is the most important aspect to release the healing agents and hence heal the cracks. This study contributes to verifying the healing efficiency of SHC and the fracture mechanism of the microcapsules. Extended finite element method (XFEM) is a flexible, and powerful discrete crack method that allows crack propagation without the requirement for re-meshing and has been shown high accuracy for modeling fracture in concrete. In this thesis, a computational fracture modeling approach of Encapsulation-based SHC is proposed based on the XFEM and cohesive surface technique (CS) to study the healing efficiency and the potential of fracture and debonding of the microcapsules or the solidified healing agents from the concrete matrix as well. The concrete matrix and a microcapsule shell both are modeled by the XFEM and combined together by CS. The effects of the healed-crack length, the interfacial fracture properties, and microcapsule size on the load carrying capability and fracture pattern of the SHC have been studied. The obtained results are compared to those obtained from the zero thickness cohesive element approach to demonstrate the significant accuracy and the validity of the proposed simulation. The present fracture simulation is developed to study the influence of the capsular clustering on the fracture mechanism by varying the contact surface area of the CS between the microcapsule shell and the concrete matrix. The proposed fracture simulation is expanded to 3D simulations to validate the 2D computational simulations and to estimate the accuracy difference ratio between 2D and 3D simulations. In addition, a proposed design method is developed to design the size of the microcapsules consideration of a sufficient volume of healing agent to heal the expected crack width. This method is based on the configuration of the unit cell (UC), Representative Volume Element (RVE), Periodic Boundary Conditions (PBC), and associated them to the volume fraction (Vf) and the crack width as variables. The proposed microcapsule design is verified through computational fracture simulations. KW - Beton KW - Bruchverhalten KW - Finite-Elemente-Methode KW - Self-healing concrete KW - Computational fracture modeling KW - Capsular clustering; Design of microcapsules KW - XFEM KW - Cohesive surface technique KW - Mikrokapsel KW - Selbstheilendem Beton KW - Computermodellierung des Bruchverhaltens KW - Entwurf von Mikrokapseln KW - Kapselclustern KW - Erweiterte Finite-Elemente-Methode KW - Kohäsionsflächenverfahren Y1 - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20221124-47467 ER - TY - THES A1 - Mansfeld, Thomas T1 - Das Quellverhalten von Alkalisilikatgelen unter Beachtung ihrer Zusammensetzung T1 - The swelling behaviour of alkali silicate gels considering their composition N2 - Im Rahmen dieser Arbeit wurden über verschiedene Herstellungsverfahren 48 Gelproben erzeugt und auf ihr Quellverhalten untersucht. Dabei wurde eine Wiederholbarkeit der Messungen mit anderen Bearbeitern überprüft und nachgewiesen. Es zeigt sich in den Quellversuchen, dass hohe Alkaligehalte in den Gelproben bei einer niedrigen Löslichkeit (durch geringe Mengen Calcium in der Probe hervorgerufen) hohe Quelldrücke erzeugen. Ein Einfluss des Natrium-Kalium-Verhältnisses (Alkaliverhältnis) auf das Quellverhalten der Gelproben ist nicht zu erkennen. Der Einfluss des Calciums im Gel zeichnet sich deutlich ab, ohne Calcium bauen die Proben keine Quelldrücke auf, bei zu hohen Calciumgehalten entstehen nicht quellfähige Alkali-Calcium-Silikat-Hydrate. Ein quellfähiger Bereich kann von ca. 5 % bis zu ca. 30 % Calciumanteil im Gel angegeben werden. Neben dem Einfluss des Calciumgehaltes auf das Quellverhalten der Gele ist auch ein Einfluss des Alkali-Silika-Verhältnisses in den Proben nachweisbar. Wird dieses Verhältnis in den Proben stark Richtung Kieselsäure verschoben, d. h. niedrige Alkalianteile im Gel, kommt es zu keinen Quellerscheinungen. Somit kann die Wirkung von AKR-vermeidenden Zusätzen (FA, Silika usw.) mit diesen Messungen bestätigt werden. Es kann gezeigt werden, dass die ermittelten Quelldrücke eines Alkalikiesel-Gels ein Gesteinskorn oder/und die umgebende Matrix zerstören können. Aus diesen oben genannten Erkenntnissen wird ein Bereich einer quellfähigen Zusammensetzung eines Gels in einem Dreistoffdiagramm angegeben und es können folgende Schlussfolgerungen gezogen werden: •Ein Quelldruck kann in einem AK-Gel nur bei einer bestimmten Menge an eingebautem Calcium aufgebaut werden. •Diese Quelldrücke können deutlich Werte über 10 N/mm² erreichen. •Die im Beton verwendeten Gesteinskörnungen und auch die sie umschließende Mörtelmatrix können mit Quelldrücken in den hier bestimmten Größenordnungen zerstört werden. •Die bekannten Modelle zur Alkali-Kieselsäure-Reaktion müssen um den Einbau des Calciums in ein entstandenes AK-Gel erweitert werden. N2 - In the context of this work over different manufacturing processes 48 gel samples were produced and examined for their swelling behaviour. A repeatability of the measurements with other editors was examined and proven. It shows up in the swelling tests that high alkali contents in the gel samples produce high swelling pressures. An influence of the sodium potassium relationship (alkali relationship) on the swelling behaviour of the gel samples is not to be recognized. The influence of the calcium in the gel appears clearly, without calcium develops the samples no swelling pressures, with to high calcium contents develops not swelling alkali calcium silicate hydrates. A swelling range can be indicated from approx 5% to approx 30% calcium content in the gel. Apart from the influence of the calcium content on the swelling behaviour of the gels also an influence of the alkali Silika relationship is in the samples provable. If this relationship in the samples is shifted strongly direction silicic acid, i.e. low alkali portions in the gel, it comes to no swelling pressure. Thus the effect of ASR avoiding additives (fly asch, silica etc.) with these measurements can be confirmed. It can be shown that the determined swelling pressures of an alkali silicate gel can destroy a rock grain and/or the surrounding matrix. From these realizations specified above a range of a pourable composition of a gel will be able to do it indicated in a three material diagram and the following conclusions to be pulled: •A swelling pressure can be developed in a alkali silcate gel only with a certain quantity of inserted calcium. •These swelling pressures can reach values over 10 N/mm². •The rock granulations used in the concrete and also the mortar matrix enclosing them can be destroyed with swelling pressures in the orders of magnitude determined here. •The well-known models for alkali silicic acid reaction must be extended by the installation of the calcium into a developed Alkali silcate gel. KW - Alkalilösliche Kieselsäure KW - Beton KW - Quellen KW - Quelldruck KW - Alkali-Kieselsäure-Reaktion KW - Alkali-Kieselsäure-Gel KW - alkali silicate gels KW - swelling KW - alkali silicate reaction Y1 - 2008 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20090106-14572 ER - TY - THES A1 - Flohr, Alexander T1 - Der Einfluss von Polymermodifikationen, unterschiedlichen Gesteinskörnungen und Gesteinskörnungssubstitutionsmaterial auf das Verformungs- und Bruchverhalten von Beton N2 - In dieser Arbeit werden die Ergebnisse von experimentellen Untersuchungen an unbewehrten und bewehrten modifizierten Betonen unter monoton steigender Belastung bis zum Bruch, einfacher Kurzzeitbelastung im Grenzbereich der Tragfähigkeit und mehrfach wiederholter Belastung mit kontinuierlicher Be- und Entlastungsgeschwindigkeit vorgestellt und ausgewertet. Für die Modifizierung der Betone wurden zwei grundsätzliche Vorgehens¬weisen angewendet: die Variation der Gesteinskörnung und die Modifizierung der Bindemittelphase mit thermoplastischen Polymeren. Die Auswirkungen der Modifikationen auf die Festigkeitseigenschaften und das Formänderungsverhalten des Betons bei Kurzzeitbelastung waren dabei von besonderem Interesse. Die beobachteten Veränderungen der Festbetoneigenschaften sowie der nichtlineare Zu-sammenhang zwischen den elastischen und nichtelastischen Verformungsanteilen signali-sieren, dass derartige Modifizierungen das Verformungs- und Bruchverhalten von Beton sig-nifikant beeinflussen und somit beim Nachweis der Tragfähigkeit und Gebrauchstauglichkeit berücksichtigt werden müssen. Neben der Evaluierung des beanspruchungsabhängigen Formänderungsverhaltens werden die etablierten Ansätze zur Beschreibung der Gefügezu-standsbereiche bei Druckbelastung weiter entwickelt, so dass die Übergänge zwischen den Bereichen exakt ermittelt und die Ausprägung der Bereiche quantifiziert werden können. Damit ist ein genauerer Vergleich der durch die Modifizierungen hervorgerufenen Verände-rungen möglich. N2 - The results of experimental investigations of unreinforced and reinforced modified concrete under monotonically increasing load until fracture, simple short-term load at the limit of capa-city and repeated load with continuous loading and release rate are introduced in the pre-sented thesis. The modification of the concretes was approached in two ways: the variation of the aggregates and the modification of the binder phase with thermoplastic polymers. Of particular interest were the effects of the modifications on the strength properties and the deformation behavior under short-term load. The observed changes in the hardened concrete properties and the non-linear relation be-tween the elastic and inelastic proportions of deformation indicate that such modifications affect the deformation and fracture behavior of concrete significantly. Therefore they have to be accounted for the analysis of capacity and suitability. In addition to the evaluation of the load-dependent deformation behavior, the established approaches to describe the structural state areas are developed further. Therewith, the transitions between the areas can be de-termined accurately and the dimension of the areas can be quantified. As a result the chang-es caused by modifications could be compared more precisely. KW - Beton KW - Polymermodifizierter Beton KW - Concrete KW - Gesteinskörnung KW - Gesteinskörnungssubstitutionsmaterial KW - Lastverformungsverhalten KW - Bruchverhalten KW - Druckbelastung KW - Zugbelastung KW - Biegezugbelastung KW - Polymermodified Cement Concrete KW - aggregates KW - deformation behavior Y1 - 2013 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20130806-20035 ER - TY - THES A1 - Giebson, Colin T1 - Die Alkali-Kieselsäure-Reaktion in Beton für Fahrbahndecken und Flugbetriebsflächen unter Einwirkung alkalihaltiger Enteisungsmittel N2 - Das Hauptziel der Arbeit war es zu klären, ob alkalihaltige Enteisungsmittel eine Alkali-Kieselsäure-Reaktion (AKR) auslösen und/oder beschleunigen können und was die dabei ggf. zugrunde liegenden Mechanismen sind. Die Untersuchungen dazu ergaben, dass die auf Verkehrsflächen eingesetzten alkalihaltigen Enteisungsmittel auf Basis von Natriumchlorid (Fahrbahndecken) bzw. auf Basis der Alkaliacetate und -formiate (Flugbetriebsflächen) den Ablauf einer AKR in Betonen mit alkalireaktiven Gesteinskörnungen auslösen und mitunter stark beschleunigen können. Dabei nimmt die AKR-fördernde Wirkung der Enteisungsmittel in der Reihenfolge Natriumchlorid - Alkaliacetate - Alkaliformiate erheblich zu. Es zeigte sich, dass im Fall der Alkaliacetate und -formiate nicht allein die Zufuhr von Alkalien von Bedeutung ist, sondern dass es außerdem zu einer Freisetzung von OH-Ionen aus dem Portlandit und folglich zu einem Anstieg des pH-Wertes in der Porenlösung kommt. Dadurch wird der Angriff auf alkalireaktives SiO2 in Gesteinskörnungen verstärkt und der Ablauf einer AKR beschleunigt. Unter äußerer NaCl-Zufuhr kommt es hingegen nicht zu einem Anstieg des pH-Wertes, was der Grund für die weniger stark AKR-fördernde Wirkung von NaCl ist. Von Bedeutung sind hier die zugeführten Na-Ionen und offenbar ein sich andeutender, direkter Einfluss von NaCl auf das SiO2-Löseverhalten. Sind pH-Wert und Na-Konzentration in der Porenlösung ausreichend hoch, wird sich thermodynamisch bedingt AKR-Gel bilden. Die Bildung von FRIEDEL’schem Salz ist dabei nur eine Begleiterscheinung, aber keine Voraussetzung für den Ablauf einer AKR unter äußerer NaCl-Zufuhr. Es zeigte sich weiter, dass sich mit der FIB-Klimawechsellagerung als Performance-Prüfung das AKR-Schädigungspotential von Betonen für Fahrbahndecken und Flugbetriebsflächen zuverlässig beurteilen lässt. Die Vorteile der FIB-Klimawechsellagerung liegen in der Prüfung kompletter, projektspezifischer Betonzusammensetzungen unter Beachtung aller praxisrelevanten klimatischen Einwirkungen und vor allem in der Berücksichtigung einer äußeren Alkalizufuhr. Innerhalb von 36 Wochen kann das AKR-Schädigungspotential einer Betonzusammensetzung für eine Nutzungsdauer von 20-30 Jahren in der Praxis sicher beurteilt werden. N2 - The primary objective of this thesis was to elucidate whether alkali-containing deicers are able to trigger and/or to accelerate an alkali-silica reaction (ASR) in concrete and, if so, what the reaction mechanisms are. The investigations showed that alkali-containing deicers used for highway (sodium chloride) and airfield (alkali acetates/formates) pavements are able to trigger and highly accelerate ASR in concrete with alkali-reactive aggregates. The aggressiveness of the deicers increases in the order sodium chloride – alkali acetates – alkali formates. The results indicate that in case of the alkali acetates and formates it is not just an issue of the alkalis but also of an additional release of OH-ions from portlandite, resulting in an increase of the pH in the concrete pore solution. Hence, the attack on silica in alkali-reactive aggregates is intensified and the ASR can be highly accelerated. For sodium chloride, however, it was evident that there is not an increase of the pH what is the decisive reason for its less severe impact on the ASR. Vitally important is the excess supply of Na-ions together with clear indications that sodium chloride is able to influence the dissolution behaviour of silica directly. Thermodynamically driven, ASR-gel will form if the pH and the Na-concentration are sufficiently high. The formation of chloroaluminates like FRIEDEL’s salt is thus rather an accompanying than a required reaction for an ASR. It could be shown furthermore that the cyclic climate storage as a performance test is able to assess the ASR potential of concrete mixtures for highway and airfield pavements reliably. The advantages of the cyclic climate storage are to test project specific concrete compositions, i.e. job mixtures, under extensively realistic conditions, including the impact of alkali-containing deicers. Within 36 weeks, it is possible to safely predict the ASR potential of the mixtures for a service life of 20-30 years. KW - Beton KW - Alkali-Kieselsäure-Reaktion KW - Alkali-Kieselsäure-Reaktion; Fahrbahndecken; Flugbetriebsflächen; äußere Alkalizufuhr; Enteisungsmittel; Natriumchlorid; Alkaliacetate; Alkaliformiate; AKR-Performance-Prüfung; FIB-Klimawechsellagerung KW - alkali-silica reaction; pavements; external alkalis; deicer; sodium chloride; alkali acetates; alkali formates; ASR performance test; cyclic climate storage Y1 - 2013 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20131217-20916 SN - 978-3-00-044366-4 (Druckversion) ER - TY - THES A1 - Voland, Katja T1 - Einfluss der Porosität von Beton auf den Ablauf einer schädigenden Alkali-Kieselsäure-Reaktion N2 - Der Dissertation liegt die Frage zugrunde, welchen Einfluss die Porosität von Beton auf den Ablauf einer schädigenden AKR hat. Insbesondere soll geklärt werden, ob der Einsatz von Gleitschalungsfertigern – anstelle von klassischen schienengeführten Betondeckenfertigern – und die damit verbundene verringerte Porosität der Betone den Ablauf einer schädigenden AKR begünstigt. Eine verringerte Porosität führt zu einer reduzierten Duktilität des Betons, so dass infolge AKR entstehende Zugspannungen schlechter abgebaut werden können. Weiterhin steht ein geringerer Expansionsraum für das entstehende AKR-Gel zur Verfügung. Diese Faktoren können den Ablauf einer AKR begünstigen. Allerdings können extern anstehende Alkalien schlechter in den Beton mit einer verringerten Porosität eindringen. Ferner wird die Diffusion der Alkalien zu den potenziell reaktiven Gesteinskörnungen verlangsamt. Zur Beantwortung der aufgeworfenen Frage wird unter Einsatz einer neuartigen Prüfmethodologie und bei variierender Porosität untersucht, welche Schädigungsparameter maßgebend für den Ablauf und die Intensität einer schädigenden AKR sind. Die berücksichtigten Schädigungsparameter sind die mechanischen Eigenschaften des Betons, der zur Verfügung stehende Expansionsraum und die im Beton ablaufenden Transportvorgänge. Um den Einfluss der jeweiligen Schädigungsparameter spezifizieren zu können, gehen die Prüfungen einerseits von einem hohen internen und andererseits von einem hohen externen AKR-Schädigungspotenzial aus. In beiden Fällen erfolgen die Untersuchungen an langsam reagierenden alkaliempfindlichen Gesteinskörnungen. Die unterschiedlichen Porositäten ergeben sich hauptsächlich durch Variation des w/z-Wertes. Bei dem hohen internen AKR-Schädigungspotenzial stehen die mechanischen Eigenschaften und der Expansionsraum im Vordergrund; außerdem ist der Einfluss der Zugabe eines LP-Bildners zu analysieren. Um ein hohes internes AKR-Schädigungspotenzial zu erreichen, kommt bei der Herstellung der Betonprobekörper ein Zement mit einem hohen Alkaligehalt zum Einsatz. Die Betonprobekörper werden der 40 °C-Nebelkammerlagerung und dem 60 °C-Betonversuch über Wasser unterzogen. Dabei findet eine neue Prüfmethodologie Anwendung, die der kontinuierlichen Messung der Dehnung und der ablaufenden Erhärtungs- und Rissbildungsprozesse dient. Diese Prüfmethodologie umfasst die Messung der Ultraschallgeschwindigkeit, die Schallemissionsanalyse und die µ-3D-Computertomografie. Hingegen richtet sich der Fokus bei dem hohen externen AKR-Schädigungspotenzial auf die Transportvorgänge. Zur Provokation eines hohen externen AKR-Schädigungspotenzials werden die Probekörper der FIB-Klimawechsellagerung ausgesetzt. N2 - This thesis deals with the question of how the porosity of concrete influences the process of a damaging alkali-silica-reaction (“ASR”). In particular, it is examined whether the use of slip form pavers and the reduced porosity resulting from this use have an effect on the process of a damaging ASR. A reduced porosity leads to a lower ductility of the concrete. Thus it is more difficult for the tensile stress to be reduced. Moreover, the space for the ASR gel to expand is reduced. These consequences promote the ASR. By contrast, the permeability of the concrete is lower. Hence, the penetration of external alkalis is reduced and the diffusion of the alkalis to the potentially reactive aggregate slowed down. An innovative non-destructive testing methodology is applied to answer this question. Based on variations of the porosity it is examined which damage parameters influence the process and intensity of a damaging ASR. The damaging parameters taken into consideration are the mechanical properties of the concrete, the expansion space and the transport processes within the concrete. In order to determine the influence of the relevant damaging parameters two categories of tests are conducted: one category is based on a high internal potential for damages due to ASR, the other one on a high external potential. In both cases alkali-reactive slow/late aggregates are tested. The different porosities of the concrete mainly result from a variation of the w/c-ratio. In case of a high internal potential for ASR-damages the mechanical properties and the expansion space play the most important role. Furthermore; the influence of an air-entraining agent on the process of a damaging ASR is taken into account. The high internal potential for ASR-damages is provoked by the use of cement with a high amount of alkalises for the production of the concrete samples. These samples are stored in the 40 °C fog chamber storage and the 60 °C concrete prisms test. On the one hand the expansion and the change in mass as well as the eigenfrequency are measured discon-tinuously in the conventional way. On the other hand the innovative testing methodology applied to these ASR-provoked stored concrete samples serves to continuously measure the expansion and the hardening as well as crack formation processes. This methodology comprises a determination of the ultrasonic velocity and of acoustic emissions as well as 3-dimensional micro X-ray computed tomography (µ-3D-CT). The high external potential for ASR-damages is provoked by the cyclic climate storage, designed by FIB. The analysis of these concretes focuses on transportation processes. KW - Alkali-Kieselsäure-Reaktion KW - Beton KW - Porosität KW - Auslaugung KW - Natriumchlorid KW - FIB-Klimawechsellagerung KW - 40 °C Nebelkammer KW - 60 °C-Betonversuch über Wasser KW - Schallemissionsanalyse KW - µ-3D Computertomografie Y1 - 2016 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:gbv:wim2-20160418-25598 ER -