@phdthesis{Mueller, author = {M{\"u}ller, Matthias}, title = {Salt-frost Attack on Concrete - New Findings regarding the Damage Mechanism}, doi = {10.25643/bauhaus-universitaet.4868}, url = {http://nbn-resolving.de/urn:nbn:de:gbv:wim2-20230103-48681}, school = {Bauhaus-Universit{\"a}t Weimar}, abstract = {The reduction of the cement clinker content is an important prerequisite for the improvement of the CO2-footprint of concrete. Nevertheless, the durability of such concretes must be sufficient to guarantee a satisfactory service life of structures. Salt frost scaling resistance is a critical factor in this regard, as it is often diminished at increased clinker substitution rates. Furthermore, only insufficient long-term experience for such concretes exists. A high salt frost scaling resistance thus cannot be achieved by applying only descriptive criteria, such as the concrete composition. It is therefore to be expected, that in the long term a performance based service life prediction will replace the descriptive concept. To achieve the important goal of clinker reduction for concretes also in cold and temperate climates it is important to understand the underlying mechanisms for salt frost scaling. However, conflicting damage theories dominate the current State of the Art. It was consequently derived as the goal of this thesis to evaluate existing damage theories and to examine them experimentally. It was found that only two theories have the potential to describe the salt frost attack satisfactorily - the glue spall theory and the cryogenic suction theory. The glue spall theory attributes the surface scaling to the interaction of an external ice layer with the concrete surface. Only when moderate amounts of deicing salt are present in the test solution the resulting mechanical properties of the ice can cause scaling. However, the results in this thesis indicate that severe scaling also occurs at deicing salt levels, at which the ice is much too soft to damage concrete. Thus, the inability of the glue spall theory to account for all aspects of salt frost scaling was shown. The cryogenic suction theory is based on the eutectic behavior of salt solutions, which consist of two phases - water ice and liquid brine - between the freezing point and the eutectic temperature. The liquid brine acts as an additional moisture reservoir, which facilitates the growth of ice lenses in the surface layer of the concrete. The experiments in this thesis confirmed, that the ice formation in hardened cement paste increases due to the suction of brine at sub-zero temperatures. The extent of additional ice formation was influenced mainly by the porosity and by the chloride binding capacity of the hardened cement paste. Consequently, the cryogenic suction theory plausibly describes the actual generation of scaling, but it has to be expanded by some crucial aspects to represent the salt frost scaling attack completely. The most important aspect is the intensive saturation process, which is ascribed to the so-called micro ice lens pump. Therefore a combined damage theory was proposed, which considers multiple saturation processes. Important aspects of this combined theory were confirmed experimentally. As a result, the combined damage theory constitutes a good basis to understand the salt frost scaling attack on concrete on a fundamental level. Furthermore, a new approach was identified, to account for the reduced salt frost scaling resistance of concretes with reduced clinker content.}, subject = {Beton}, language = {en} } @phdthesis{Mueller, author = {M{\"u}ller, Matthias}, title = {Frost-Tausalz-Angriff auf Beton - Neue Erkenntnisse zum Schadensmechanismus}, doi = {10.25643/bauhaus-universitaet.4502}, url = {http://nbn-resolving.de/urn:nbn:de:gbv:wim2-20210922-45025}, school = {Bauhaus-Universit{\"a}t Weimar}, pages = {226}, abstract = {F{\"u}r die Verminderung der betonspezifischen CO2-Emissionen wird ein verst{\"a}rkter Einsatz klinkerreduzierter Zemente bzw. Betone angestrebt. Die Reduzierung des Klinkergehaltes darf jedoch nicht zu einer lebensdauerrelevanten Beeintr{\"a}chtigung der Betondauerhaftigkeit f{\"u}hren. In diesem Zusammenhang stellt der Frost-Tausalz-Widerstand eine kritische Gr{\"o}ße dar, da er bei h{\"o}heren Klinkersubstitutionsraten h{\"a}ufig negativ beeinflusst wird. Erschwerend kommt hinzu, dass f{\"u}r klinkerreduzierte Betone nur ein unzureichender Erfahrungsschatz vorliegt. Ein hoher Frost-Tausalz-Widerstand kann daher nicht ausschließlich anhand deskriptiver Vorgaben gew{\"a}hrleistet werden. Demgem{\"a}ß sollte perspektivisch auch f{\"u}r frost-tausalzbeanspruchte Bauteile eine performancebasierte Lebensdauerbetrachtung erfolgen. Eine unverzichtbare Grundlage f{\"u}r das Erreichen dieser Ziele ist ein Verst{\"a}ndnis f{\"u}r die Schadensvorg{\"a}nge beim Frost-Tausalz-Angriff. Der Forschungsstand ist jedoch gepr{\"a}gt von widerspr{\"u}chlichen Schadenstheorien. Somit wurde als Zielstellung f{\"u}r diese Arbeit abgeleitet, die existierenden Schadenstheorien unter Ber{\"u}cksichtigung des aktuellen Wissensstandes zu bewerten und mit eigenen Untersuchungen zu pr{\"u}fen und einzuordnen. Die Sichtung des Forschungsstandes zeigte, dass nur zwei Theorien das Potential haben, den Frost-Tausalz-Angriff umfassend abzubilden - die Glue Spall Theorie und die Cryogenic Suction Theorie. Die Glue Spall Theorie f{\"u}hrt die Entstehung von Abwitterungen auf die mechanische Sch{\"a}digung der Betonoberfl{\"a}che durch eine anhaftende Eisschicht zur{\"u}ck. Dabei sollen nur bei moderaten Tausalzkonzentrationen in der einwirkenden L{\"o}sung kritische Spannungszust{\"a}nde in der Eisschicht auftreten, die eine Sch{\"a}digung der Betonoberfl{\"a}che hervorrufen k{\"o}nnen. In dieser Arbeit konnte jedoch nachgewiesen werden, dass starke Abwitterungen auch bei Tausalz¬konzentrationen auftreten, bei denen eine mechanische Sch{\"a}digung des Betons durch das Eis auszuschließen ist. Damit wurde die fehlende Eignung der Glue Spall Theorie aufgezeigt. Die Cryogenic Suction Theorie fußt auf den eutektischen Eigenschaften von Tausalz-l{\"o}sungen, die im gefrorenen Zustand immer als Mischung auf festem Wassereis und fl{\"u}ssiger, hochkonzentrierter Salzl{\"o}sung bestehen, solange ihre Eutektikumstemperatur nicht unter¬schritten wird. Die fl{\"u}ssige Phase im salzhaltigen Eis stellt f{\"u}r gefrorenen Beton ein bisher nicht ber{\"u}cksichtigtes Fl{\"u}ssigkeitsreservoir dar, welches trotz der hohen Salzkonzentration die Eisbildung in der Betonrandzone verst{\"a}rken und so die Entstehung von Abwitterungen verursachen soll. In dieser Arbeit wurde best{\"a}tigt, dass die Eisbildung im Zementstein beim Gefrieren in hochkonzentrierter Tausalzl{\"o}sung tats{\"a}chlich verst{\"a}rkt wird. Das Ausmaß der zus{\"a}tzlichen Eisbildung wurde dabei auch von der F{\"a}higkeit des Zementsteins zur Bindung von Chloridionen aus der Tausalzl{\"o}sung beeinflusst. Zusammenfassend wurde festgestellt, dass die Cryogenic Suction Theorie eine gute Beschreibung des Frost-Tausalz-Angriffes darstellt, aber um weitere Aspekte erg{\"a}nzt werden muss. Die Ber{\"u}cksichtigung der intensiven S{\"a}ttigung von Beton durch den Prozess der Mikroeislinsenpumpe stellt hier die wichtigste Erweiterung dar. Basierend auf dieser {\"U}berlegung wurde eine kombinierte Schadenstheorie aufgestellt. Wichtige Annahmen dieser Theorie konnten experimentell best{\"a}tigt werden. Im Ergebnis wurde so die Grundlage f{\"u}r ein tiefergehendes Verst{\"a}ndnis des Frost-Tausalz-Angriffes geschaffen. Zudem wurde ein neuer Ansatz identifiziert, um die (potentielle) Verringerung des Frost-Tausalz-Widerstandes klinkerreduzierter Betone zu erkl{\"a}ren.}, subject = {Beton}, language = {de} } @misc{Ansari, type = {Master Thesis}, author = {Ansari, Meisam}, title = {Simulation methods for functional and microstructured composite materials}, doi = {10.25643/bauhaus-universitaet.4278}, url = {http://nbn-resolving.de/urn:nbn:de:gbv:wim2-20201103-42783}, school = {Bauhaus-Universit{\"a}t Weimar}, pages = {110}, abstract = {In this thesis, a generic model for the post-failure behavior of concrete in tension is proposed. A mesoscale model of concrete representing the heterogeneous nature of concrete is formulated. The mesoscale model is composed of three phases: aggregate, mortar matrix, and the Interfacial Transition Zone between them. Both local and non-local formulations of the damage are implemented and the results are compared. Three homogenization schemes from the literature are employed to obtain the homogenized constitutive relationship for the macroscale model. Three groups of numerical examples are provided.}, subject = {Simulation}, language = {en} } @phdthesis{Oucif, author = {Oucif, Chahmi}, title = {Analytical Modeling of Self-Healing and Super Healing in Cementitious Materials}, doi = {10.25643/bauhaus-universitaet.4229}, url = {http://nbn-resolving.de/urn:nbn:de:gbv:wim2-20200831-42296}, school = {Bauhaus-Universit{\"a}t Weimar}, pages = {208}, abstract = {Self-healing materials have recently become more popular due to their capability to autonomously and autogenously repair the damage in cementitious materials. The concept of self-healing gives the damaged material the ability to recover its stiffness. This gives a difference in comparing with a material that is not subjected to healing. Once this material is damaged, it cannot sustain loading due to the stiffness degradation. Numerical modeling of self-healing materials is still in its infancy. Multiple experimental researches were conducted in literature to describe the behavior of self-healing of cementitious materials. However, few numerical investigations were undertaken. The thesis presents an analytical framework of self-healing and super healing materials based on continuum damage-healing mechanics. Through this framework, we aim to describe the recovery and strengthening of material stiffness and strength. A simple damage healing law is proposed and applied on concrete material. The proposed damage-healing law is based on a new time-dependent healing variable. The damage-healing model is applied on isotropic concrete material at the macroscale under tensile load. Both autonomous and autogenous self-healing mechanisms are simulated under different loading conditions. These two mechanisms are denoted in the present work by coupled and uncoupled self-healing mechanisms, respectively. We assume in the coupled self-healing that the healing occurs at the same time with damage evolution, while we assume in the uncoupled self-healing that the healing occurs when the material is deformed and subjected to a rest period (damage is constant). In order to describe both coupled and uncoupled healing mechanisms, a one-dimensional element is subjected to different types of loading history. In the same context, derivation of nonlinear self-healing theory is given, and comparison of linear and nonlinear damage-healing models is carried out using both coupled and uncoupled self-healing mechanisms. The nonlinear healing theory includes generalized nonlinear and quadratic healing models. The healing efficiency is studied by varying the values of the healing rest period and the parameter describing the material characteristics. In addition, theoretical formulation of different self-healing variables is presented for both isotropic and anisotropic maerials. The healing variables are defined based on the recovery in elastic modulus, shear modulus, Poisson's ratio, and bulk modulus. The evolution of the healing variable calculated based on cross-section as function of the healing variable calculated based on elastic stiffness is presented in both hypotheses of elastic strain equivalence and elastic energy equivalence. The components of the fourth-rank healing tensor are also obtained in the case of isotropic elasticity, plane stress and plane strain. Recent research revealed that self-healing presents a crucial solution also for the strengthening of the materials. This new concept has been termed ``Super Healing``. Once the stiffness of the material is recovered, further healing can result as a strengthening material. In the present thesis, new theory of super healing materials is defined in isotropic and anisotropic cases using sound mathematical and mechanical principles which are applied in linear and nonlinear super healing theories. Additionally, the link of the proposed theory with the theory of undamageable materials is outlined. In order to describe the super healing efficiency in linear and nonlinear theories, the ratio of effective stress to nominal stress is calculated as function of the super healing variable. In addition, the hypotheses of elastic strain and elastic energy equivalence are applied. In the same context, new super healing matrix in plane strain is proposed based on continuum damage-healing mechanics. In the present work, we also focus on numerical modeling of impact behavior of reinforced concrete slabs using the commercial finite element package Abaqus/Explicit. Plain and reinforced concrete slabs of unconfined compressive strength 41 MPa are simulated under impact of ogive-nosed hard projectile. The constitutive material modeling of the concrete and steel reinforcement bars is performed using the Johnson-Holmquist-2 damage and the Johnson-Cook plasticity material models, respectively. Damage diameters and residual velocities obtained by the numerical model are compared with the experimental results and effect of steel reinforcement and projectile diameter is studied.}, subject = {Schaden}, language = {en} } @phdthesis{Flohr, author = {Flohr, Alexander}, title = {Der Einfluss von Polymermodifikationen, unterschiedlichen Gesteinsk{\"o}rnungen und Gesteinsk{\"o}rnungssubstitutionsmaterial auf das Verformungs- und Bruchverhalten von Beton}, doi = {10.25643/bauhaus-universitaet.2003}, url = {http://nbn-resolving.de/urn:nbn:de:gbv:wim2-20130806-20035}, school = {Bauhaus-Universit{\"a}t Weimar}, pages = {148}, abstract = {In dieser Arbeit werden die Ergebnisse von experimentellen Untersuchungen an unbewehrten und bewehrten modifizierten Betonen unter monoton steigender Belastung bis zum Bruch, einfacher Kurzzeitbelastung im Grenzbereich der Tragf{\"a}higkeit und mehrfach wiederholter Belastung mit kontinuierlicher Be- und Entlastungsgeschwindigkeit vorgestellt und ausgewertet. F{\"u}r die Modifizierung der Betone wurden zwei grunds{\"a}tzliche Vorgehens¬weisen angewendet: die Variation der Gesteinsk{\"o}rnung und die Modifizierung der Bindemittelphase mit thermoplastischen Polymeren. Die Auswirkungen der Modifikationen auf die Festigkeitseigenschaften und das Form{\"a}nderungsverhalten des Betons bei Kurzzeitbelastung waren dabei von besonderem Interesse. Die beobachteten Ver{\"a}nderungen der Festbetoneigenschaften sowie der nichtlineare Zu-sammenhang zwischen den elastischen und nichtelastischen Verformungsanteilen signali-sieren, dass derartige Modifizierungen das Verformungs- und Bruchverhalten von Beton sig-nifikant beeinflussen und somit beim Nachweis der Tragf{\"a}higkeit und Gebrauchstauglichkeit ber{\"u}cksichtigt werden m{\"u}ssen. Neben der Evaluierung des beanspruchungsabh{\"a}ngigen Form{\"a}nderungsverhaltens werden die etablierten Ans{\"a}tze zur Beschreibung der Gef{\"u}gezu-standsbereiche bei Druckbelastung weiter entwickelt, so dass die {\"U}berg{\"a}nge zwischen den Bereichen exakt ermittelt und die Auspr{\"a}gung der Bereiche quantifiziert werden k{\"o}nnen. Damit ist ein genauerer Vergleich der durch die Modifizierungen hervorgerufenen Ver{\"a}nde-rungen m{\"o}glich.}, subject = {Beton}, language = {de} } @phdthesis{Ressel2004, author = {Ressel, Oliver}, title = {Entscheidungshilfen f{\"u}r die Planung von Anlagen zum naßmechanischen Recycling von Betonrestmassen}, doi = {10.25643/bauhaus-universitaet.79}, url = {http://nbn-resolving.de/urn:nbn:de:gbv:wim2-20040511-831}, school = {Bauhaus-Universit{\"a}t Weimar}, year = {2004}, abstract = {Trotz der weiten Verbreitung erfolgt die Planung der Restbetonrecyclinganlagen immer noch durch learnig-by-doing, da verfahrenstechnisches Grundlagenwissen nicht vorliegt. Wer an verantwortlicher Stelle die Investition in eine neue oder in die Verbesserung einer bestehenden Restbetonrecyclinganlage beurteilen soll, steht vor einer komplexen Entscheidung, die unter Ber{\"u}cksichtigung unterschiedlichster Kriterien getroffen werden muss. In der Praxis besteht hinsichtlich der Qualit{\"a}tssicherung der Recyclingprodukte, der Ablagerungen der noch reaktiven Zementpartikel, der Bemessung der eingesetzten Maschinen, der praktikablen Handhabung hinsichtlich einiger Detailprobleme sowie der Anordnung der verfahrenstechnischen Komponenten in Bezug zur Gel{\"a}ndeoberkante weitgehend Unklarheit. Das allgemeine Verlangen nach einer durchdachten Entscheidungshilfe und die Notwendigkeit, zu einem sachlich begr{\"u}ndeten Urteil zu kommen, macht Entscheidungshilfen f{\"u}r die Planung von Restbetonrecyclinganlagen erforderlich. Insbesondere da Fehlentscheidungen nicht nur mit großem Aufwand r{\"u}ckg{\"a}ngig gemacht werden k{\"o}nnen. Hierf{\"u}r wurden 18 maßgebliche Entscheidungskriterien entwickelt. Diese Entscheidungskriterien wurden im Rahmen der Nutzwertanalyse als Projektziele entwickelt. Die erarbeiteten Kriterien einteilen: - Kriterien zur Qualit{\"a}tssicherung bei der Verwendung der Recyclingprodukte F{\"u}r die Wiederverwendung der Recyclingprodukte Restwasser und Restbetonzu- schlag sind im technischen Regelwerk Verfahrensweisen vorgechrieben. Hinsichtlich der Prozesse bei der Wiederverwendung konnten deutliche Ver- besserungspotentiale aufgezeigt werden. Besonders die Anwendung von online- Dichtemessverfahren im Vergleich zur Ar{\"a}ometermessung verbessert die Len- kungsprozesse zur Qualit{\"a}tssicherung. Aber auch die weitere Klassierung oder das getrennte Lagern und Dosieren des Restbetonzuschlags im Vergleich zu der im technischen Regelwerk vorgeschriebenen Verfahrensweise des volumetrischen Absch{\"a}tzens bringt Verbesserungspotential. - Kriterien zur Minimierung von Ablagerungen Noch reaktive Zementpartikel kommen zeitweise permanent mit Anlagen- komponenten, Leitungen und Beckeninnenfl{\"a}chen der Recyclinganlage in Be- r{\"u}hrung. Ablagerungen von Zementpartikeln, die den Betrieb der Anlage be- hindern, verschlechtern oder sogar verhindern, sind unvermeidbar. Aller- dings kann, wie im Rahmen dieser Arbeit gezeigt wurde, eine Minimierung der Ablagerungen durch geeignete Maßnahmen herbeigef{\"u}hrt werden. Die Ablage- rungen im Suspensionsbeckenlassen sich durch den Zustand der homogenen Suspension sowie durch das Str{\"o}mungsbild angepasste Formgebung minimieren. Durch die geeignete Gef{\"a}llewahl und vor allem durch die korrekte Wahl der Pumpenart k{\"o}nnen die Ablagerungen in Leitungen minimiert werden. - Kriterien zur Bemessung der verfahrenstechnischen Apparate Die Auslegung der Recyclinganlage hinsichtlich der Auswaschleistung, der R{\"u}hrerleistung und der Gr{\"o}ße des Suspendierraumes erfolgt bisher anhand von praktischen Erfahrungswerten. In dieser Arbeit wurde f{\"u}r die Auswasch- leistung ein allgemeing{\"u}ltiges Berechnungsmodel hergeleitet. Dar{\"u}ber hinaus wurde gezeigt, dass die R{\"u}hrerleistung f{\"u}r das Suspendieren von Restwasser berechnet werden kann. Die Gr{\"o}ße des Suspendierraumes kann unter Be- r{\"u}cksichtigung der zu- und abfließenden Materialstr{\"o}me berechnet werden. Das Trennverhalten des mechanischen Klassierers wurde im Rahmen einer Ver- suchsreihe mit folgenden Ergebnissen ermittelt: a. Die Klassierdurchs{\"a}tze steigen mit gr{\"o}ßer werdendem Entleerdurchsatz. ufgrund der Pufferwirkung des mechanischen Klassierers, bei der die diskontinuierlich in den Aufgabetrichter gef{\"u}llte Restbetontr{\"u}be (Ent- leeren) in einem kontinuerlichen Prozess (Klassieren) durch den Trog gef{\"o}rdert wird, n{\"a}hert sich der Klassierdurchsatz asymtotisch einem Grenzwert an. b. Das Masseausbringen rbz wird signifikant vom Klassierdurchsatz und weniger vom Entleerdurchsatz beeinflusst. c. Die Korngr{\"o}ßenverteilung des Restbetons, des Restbetonzuschlags und des Restwassers belegen anschaulich den erreichten Trenneffekt. d. Die Trennkorngr{\"o}ße steigt mit zunehmendem Klassierdurchsatz an. Diese Tendenz ist allerdings nur bei Betrachtung des "nassen" Klassier- durchsatzes signifikant erkennbar. Bei Betrachtung des "trockenen" Durchsatzes ergibt sich keine Abh{\"a}ngigkeit. Die Ursache hierf{\"u}r ist, dass in den "nassen" Durchsatz Prozesse wie Tr{\"u}beagitation und Feinkorn- konzentration indirekt eingehen. e. Der Fehlkornanteil < 125 µm im Restbetonzuschlag steigt ebenfalls mit "nassem" Klassiersatz an. f. Im Unterschied dazu bestehen f{\"u}r den Fehlkornanteil > 125 µm im Rest- wasser signifikante Abh{\"a}ngigkeiten zu Entleer- und Klassierdurchs{\"a}tzen. Ursache ist der tote Fluss. - Kriterien zur Praktikabilit{\"a}t des Anlagenberiebes - Interdependenzen zwischen Anlagenkomponenten}, subject = {Restbeton}, language = {de} }